Subject: Chemically machining cast iron end housings
From: Paul
Date: 2/11/1999, 2:21 PM
To: z

Mark Steitle wrote:

 
Have you tried a swimming pool supply house.  I think they carry hydrochloric acid for pool treatment.
Mark

Thanks Mark.

BTW as I recall heating it speeds up the reaction.

I notice just putting the back housing on a flat
surface and pouring the acid in seems to work.
When the core plugs are gone you know you have eaten out
at least a 1/16 of an inch all around :-) 

Don't
under estimate that. It is a lot of water jacket volume
and quite a little weight.

Paul Lamar
 
The Aircraft Rotary Engine Newsletter.              Powered by Linux.

http://home.earthlink.net/~rotaryeng/            http://www.linux.org