Subject: Grooves in rotor housing water jackets.
From: Paul
Date: 6/5/1999, 11:23 AM
To: zz

JMLBlues@aol.com wrote:

Whoa! What is the experience base on grooving the rotor housing as deeply as
the steel liner???

I would be *very* concerned that this depth of grooving will significantly
weaken the housing structure. The steel is relatively thin, and thus does not
contribute significantly to the strength or stiffness of the rotor housings.
All the combustion pressure loading must be carried by the panels in the
rotor housing and transmitted via friction to the end housings where the
force "loop" is closed by the main bearing reactions. Cutting deep channels
into the rotor housing may also set up many stress concentrations leading to
fatigue failures. I am aware that the grooving is a common high performance
technique for improving heat transfer from the trochoid, but at what depth
and for what length of continuous high load operation?

Also, the grooves will do nothing to keep the housing cool in the event of
steam pocket formation.

Close to thirty years Jon. You are NOT doing it???? :-)
No noticeable or documented  bad effects so far.

Everett Hatch tried restoring some of the strength with bolt
columns from the outer water jacket with inconclusive results. 

The groves are not very long as the tension bolt bosses support
the inner housing from place to place. The longest groove
I measure is 1.25 inch while the panel is about three inches
wide. The grooves run parralel to rotor motion.  I suspect 
the effect on stress and deflections is minimal.

Have you calculated the deflection and stress both with and without
the grooves? Bruin's Analysis & Design of Flight Vehicle Structures
has some data and formulas on panels under pressure if anybody
is interested.
 
Paul Lamar
 