Subject: New end housings. R&D on housing shringage.
From: Paul
Date: 9/7/1999, 2:24 PM
To: zz

X-Mozilla-Keys:                                                                                 
Jeff Spitzer wrote:

At 03:13 PM 9/5/99 -0700, you wrote:

Paul .... That is a great idea .  Thanks .        JIM



The aluminum tube trick is only valid if the proper material is used.  Good
luck finding any 356 tube.  I suggest the substitution of something like
6063 or some "non-structural" alloy.  6061 will not be a valid test.

Jeff Spitzer

One could cut up a scrap rotor housing. We all have them lying around.

Paul Lamar
 
The Aircraft Rotary Engine Newsletter.              Powered by Linux.

http://home.earthlink.net/~rotaryeng/            http://www.linux.org