Ed Anderson wrote:
I agree with Paul, I can't see how that would cause a crack in the Hayes
Teflon "O" rings. They appeared considerably more robust, with their
silicon core and Teflon sheating, than the stock 'O' rings, by far. When I
flew my aircraft from Virginia to North Carolina on one of those 100F days
this summer. The oil temps were up to the 210F redline and above for two
hours during the flight (that's what finally decided me to switch to the
chin oil cooler location) and the coolant as a result was pushing 200-205F.
Given the results thus far, I would not hesitate to use the Hayes High
Performance 'O' rings again.
Ed Anderson