At 11:26 AM 12/9/98 -0800, you wrote:
No I am not sure but the yeild strength of the aluminum goes
down with temp. I am also not sure at what temp this might
ocurr. I will have to look up the table of aluminum yeild
strength as a function of temp. I know the fatique life is half
at 500 degrees F. [PL]
If you can't find what you're looking for I can send you some charts from
Mil-HDBK-5. The decrease of strength with temp and temp*time is more than
most people think. 7075 is no stronger than 6061 at 200 deg F IIRC due to
faster drop with temp.
Jeff Spitzer
Our temp data crossed in the email. See my 12:15 PM post.
This temperature degradation evidense supports my theory.
Also the data from the racers in Australia having trouble with
the alloy end housings. This is the message I received on
the subject.[PL]
G'day Paul.
Just wanted to let the group know to be careful with the RB aluminium
side plates. ( Nothing personal here Jim ) The expansion rate of the
side plates vary with respect to the rotor housings due to the larger
working area of the plates. Some race teams that have purchased the RB
side plates have found the engine makes power for only a limited time
then starts leaking. However, I am unsure of whether this occurs at
below 100% load. Another drawback is supposed to be the working area
itself, apparently the coating has been found to lack the required
durability for sustaned useage (under racing conditions).
Obviously all this is under the sustained 100% load of full race
engines thus I suggest you all make your own conclusions. Personally I
think it's a great product that just needs a bit more work to get it
right.
REgards Dave Morris
This is a real old message I found on the ACRE NL CD.
This is one of my main arguments for the steel side plates.
Paul Lamar
The Aircraft Rotary Engine Newsletter. Powered by Linux.
http://home.earthlink.net/~rotaryeng/ http://www.linux.org