Subject: Nickasil aluminum end housings.
From: Paul
Date: 2/10/2000, 2:42 PM

Howard Wilkinson wrote:

Paul:
    This discussion of surface treatments for wear is of considerable
interest to me as I am intending to do my own side housing castings.....  I
propose something like this....   Use Vega block high SI aluminum with the
chilled faces on the molds as described in a message earlier.... Then do a
hard anodize process on this face.  Anodizing is done with an acid bath and
an electric current.... the lower the acid strength the higher the hardness
of the anodizing.  Simple battery acid is used, or chromic or phosphoric
acid... the process is simple and doesn't require high power or
anything...... I have a good description of it in my Chemical Formulary.

One of the things you need to watch out for with any coating on aluminum
is overheating. If the surface is overheated it will corrode and pit
regardless of the coating I suspect. I have seen these pits and they are
quite deep. As much as 1/16 th of an inch.
This can be seen on aluminum cylinder heads on automotive engines
that have been run at too high of an average power level. Jeff Aucklund
of big block Chev V8 fame saw that on his cylinder heads. That is about the
time he switched over to the Czech copy PT6 turbo prop.
I also suspect this is why you never see aluminum cylinder heads on 
heavy duty truck engines. Back in WW II B29 R3350 engines were changed out
if this pitting was noticed in the exhaust ports.
Lots of factors could be involved. Perhaps there was some undetected
detonation. Perhaps some inadequate local cooling problems.