Subject: Alumiunm end housings
From: Paul
Date: 2/14/2000, 8:40 PM



There were three reasons Deere, et. al. did not try the steel/aluminum rotor
housing approach -- first was tooling cost. Mazda uses a die casting process
that better lends itself to securing the steel liner. Deere, CW and RPI
hadn't gotten to the point of a truly final configuration nor were high
volume applications envisioned. Thus, the die casting tooling costs would
have been prohibitive. Second, it was feared (backed up by analysis) that the
steel liner would be too much of a thermal barrier and raise the surface
temperatures beyond where it was thought lubrication would survive. This was
not proven by any testing, because there was no way steel liners would be
used anyway. Lastly, it was felt that chrome plating was an inadequate
coating for the stresses of stratified charge. I personally agree with this
thinking. The bond strength of chrome plating is nowhere near the bond
strength of detonation gun coatings. High mileage Mazda auto engines
frequently have some chrome missing. Under constant duty stratified charge
use, chrome would never hold up. The main reason Mazda uses the steel liner
is to facilitate applying the chrome. Chrome does not adhere well to
aluminum, and even intermediate nickel "strikes" are poorer than chrome on
steel. So, Mazda came up with a very ingenious method to use chrome plating
in a high volume application. A different set of circumstances from the Deere
military application targets.
Jon

The Aircraft Rotary Engine Newsletter.              Powered by Linux.

http://home.earthlink.net/~rotaryeng/            http://www.linux.org