Subject: aluminum tube bending
From: Paul
Date: 7/12/2000, 3:46 PM

Gary Wolf wrote:

Paul,
   Your observation about bending aluminum tubing is correct. When the
muffler shops bend it it is crude in appearance but it does the job if the
size is chosen to allow for the reduction in cross-sectional area in the
bent part. The problem with muffler shop bends is that there is no internal
filler to maintain the diameter.

   I have a mandrel bender that I use for manufacturing exhaust systems and
I generally shudder when people ask me to bend aluminum tubing for water
pipes on formula cars. The problem is that I do a draw bend that works on
steel tube but aluminum will frequently split as it passes the end of the
internal mandrel. I have seen beautiful bends on vintage Lotuses and Lolas
but have not been able to duplicate them. If anyone knows how they were
achieved, I and many others would appreciate knowing.

                                                                Gary Wolf

I'll bet they warm it up to 500 degrees or so, maybe higher as a guess.
They may also get it in the O condition. I vaguely recall that if
you heat aluminum with a torch that leaves a bunch of black carbon on
it then it is annealed. Another way is load it with lead shot and
weld the ends close. Then bend it. If you get it figured out
let me know and we will send you a bunch of work. Intake manifolds
and water pipes. What size dies do you have?

Paul Lamar
 
The Aircraft Rotary Engine Newsletter.              Powered by Linux.

http://home.earthlink.net/~rotaryeng/            http://www.linux.org