Subject: aluminum tube bending
From: Paul
Date: 7/12/2000, 8:02 PM


Paul... The trick is to take a gas torch and produce a carburizing flame. Take
that flame and coat the aluminiun with it. After you have done that, change
your torch back to a slightly less than fully feathered flame and burn the
carbon off. That should pretty well anneal the aluminium.  That is also the
way you can pre-heat an aluminium casting or thick aluminium stock prior to
T.I.G. welding so you don't add a lot of misplaced heat which would distort
the part.      JIM DANA

Thanks Jim. We need to try that on an aluminum tube bender.

Paul Lamar

Bulent Aliev wrote:

We need a spy inside Burns. They bend some amazing stuff from aluminum and there is
no carbon on the bends, but lots of lubricant  and drag marks on the inside. I
think they are dragging a ball inside the tube to keep the dimensions correct?

 
The Aircraft Rotary Engine Newsletter.              Powered by Linux.

http://home.earthlink.net/~rotaryeng/            http://www.linux.org