Subject: Bending tubing & cerrobend etc
From: Paul
Date: 7/16/2000, 5:59 PM

Scott Gettings wrote:

The composite option here is also of interest to me.  Using G-10 phenolic for a
flange, you should be able to withstand 300 degrees.  Whether this could bolt
directly onto the block or a short metal "pretube" might be necessary  to drop the
temp some is unknown.

The complex curves might could be more easily handled than doing this in metal, as
long as a two-piece mold could be used to build a "top" and "bottom" half of the
manifold.  These two halves could then be bonded to the flanges and to each other to
close it up.  Using carbon fiber and hi-temp epoxy should give plenty of heat
resistance.  One could also use a lost-foam or lost-wax technique, by carving out
the one-time shape, covering it with CF/epoxy, and then melting out the core.
Although the wax is usually a once-only scenario, you can also cast a two-piece
plaster or glass mold from the wax and use it to make more disposable plugs.  Having
a mold to pop out plugs or final products would allow production on some reasonable
scale.

Scott Gettings


 
The Aircraft Rotary Engine Newsletter.              Powered by Linux.

http://home.earthlink.net/~rotaryeng/            http://www.linux.org