Scott Gettings wrote:
I might be interested in playing with some molding techniques to see what could be
done. I would need at least a simple drawing of the desired specifications,
however. It should not be very hard to bond a flange out of G-10 phenolic on the
upper end of a composite intake system to bolt to the throttle body, as well as
the lower intake manifold (if one did not want a butt pipe-to-pipe connection).
Really tough stuff and good to 300 degrees. A composite tube might crush with a
clamping load, although one end could easily be beefed up by adding more layers.
With the lost-wax technique, the inside of the manifold would be smooth (as smooth
as the wax) but the outside unfinished. Functional but not necessarily pretty.
Carbon fiber and hi-temp epoxy could wrap around each pipe to form a seamless
chamber. On the other hand, creating a two-piece mold with a top and bottom of
all the tubes together should be feasible, which could result in flat sections
between/around each tube to bond together and provide mounting points. Might be
some limitations if the curves were too complex to pull out of a multi-piece mold,
however. I'd vacuum bag each half, then bond the two halves and any flanges
together. This would result in a perfect outside finish, and a relatively smooth
inside finish, too. Once the molds were done, it should be easy to mass-produce.
If Paul or anyone else thinks this might be worthwhile and wants to post some
drawings, I'll see what I can do (no guarantees, for sure!).
Regarding the styrofoam technique, I'm not sure how one would handle the inside of
curved tubes using a "lost foam" technique and cast metal. The outside could be
done in plaster, but it might be very hard to get out of the inside of the tube.
Dissolve it in acid?
Scot Gettings
Gasoline or acidtone dissolves styrofoam. I was thinking a hand layup over
the male styrofoam mold.
Paul Lamar