Here is what Tracy's kludged up, temporary, mild steel muffler pipes looked
like
after only a few hours of flying on his way out to Copper State.
Tracy says a thin part of the surface would flake off after each
thermal cycle. Stainless steel if not Inconel is essential for these parts.
Paul Lamar
Chuck Dunlap wrote:
Y pipes are .100 wall mild steel from Racing Beat. They were flaking a lot at
first but seem to have slowed down a lot now. I have 70 hours on it. I
wonder if the chemistry of the metal is changing. One of my welds cracked at
60 hours and I had to remove and re-weld it.I estimate another 70 hours and
they will be finished and ready for plan B!
Chuck Dunlap