Hi Guys;
Yep,------Splicing SOLID non Teflon o-rings works
great, especially if you scarf the ends 45 deg. The
joint in most cases is stronger than the
rest...........But, don't even think about doing this
with a Teflon coated o-rings.......what WILL happen is
the Teflon covering will eventually break the bond and
provide an opening for fluid to get thru.
We learned this the hard way in the chemical and
pharmaceutical equipment industry. (1.3 million dollar
lesson)
Of course, if there is some new hi-tech super duper
bonding agent that bonds to Teflon as well as the inner
material (I doubt it) out there, by all means give it a
shot.........Just remember that if it harms the inner
material it would be just as bad, as it would cause the
Teflon coating to collapse.
The best thing is to keep on searching for the correct
size, if you want to try a slightly larger one freeze it
before installation. If it doesn't shrink enough, try
heating it in the oven and compress it in place.
This is how we did it on our equipment.
I've been following this closely and I would say you are
95% THERE so don't give up.
Butch
The AirCraft Rotary Engine NewsLetter. Powered by Linux.