Subject: Chuck Dunlaps oil cooling and muffler.
From: ACRE NL
Date: 6/20/2001, 8:47 AM


As I recall Chuck told me this simple sheet aluminum fairing
made a large improvement in his oil temps. Is that correct
Chuck?

The exhaust pipe coming out of the muffler looks a bit on the
small side. Also you might try doing away with that Y in the
down pipes and going into the muffler with two separate pipes.
Could have some back pressure going on there.

How is that muffler holding up Chuck?

Paul Lamar


Yes the fairing made a BIG difference. The oil went up to 230 F on the first
flight, even though throttled way back after liftoff. With the duct fairings
added, have never seen oil over my limit of 220F.

I had to weld up a crack at the muffler inlet at about 20 hours, no problems
since then. About 130 hours on the muffler so far.

I am making a new SS downpipe header. The present one is .100" wall mild
steel from Racing Beat and seems like a little more wall material flakes off
every time it runs. My welds have cracked twice in 155 hours. The Y design
makes the header a solid assembly so if there is a crack, the pipe cannot
move anywhere and cause a hazard. Of course the solid design also puts more
stress on the welds as it heats and expands. The new header has slip joints.
The Y collector on the new header is a bit larger so may have less back
pressure. I could have redesigned it, but then would have to make a new
muffler, new mounting arrangement. etc. If you change one thing, you have to
change 10 others!

Chuck Dunlap