> >From discussions with those with carbon experience is that hand lay-up of
carbon
is not a desirable way to go due to the fact you can't guaranteed consistant
outcomes
in strength . However I have seen much in the way of manufactured
carbon tube under 'controlled conditions', perhaps someone can do what you
> need or can supply ex-stock.
James Russell wrote:
Hi all:
If you could find someone to filament wind carbon tape on your AL core ( with
a ply of 120 glass first ), and cure at 250 F. That way the fibers
would be running
+/- 45 for torsion with some plys at + 90...
Or, handwrap prepreg tape w/ alot of debulking stages before the final cure in
a Rutan-style metal box w/ a house furnace heater or an old pizza
oven... Heat shrink tape squeezes from the outside while the
expansion of the AL tube helps from the
inside. I would release the tube as a tool, and PAA another like tube
to bond in after
cure for the final part.
It's more fun to lay-up your own parts, but manfactured ones would
probably have
less voids...
Just a thought...
Regards,
James