Subject: PSRU plate motor mount stress
From: ACRE NL
Date: 7/10/2001, 7:56 PM


This plate as is... is way overkill.

The idea is to come in from both sides the same .2" amount to
minimize
residual stress warping. Leave about .1 inch thick web and scale
it off this drawing. If that proves to be bothersome I will add

"Kevin R. Walsh" wrote:

Be very careful here.  A part that is statically way overbuilt will
[could] fail dynamically.  When putting those pockets in, you MUST use a
radiused end mill.  Otherwise the sharp corner is a stress riser and you
will [may] have cracks.  Aluminum already has poor fatigue life.  Dont make
the problem worse by adding crack starts.


Kevin Russert Walsh
Sr. Process & Equipment Development Engineer

"Could" and "may" Kevin.  Not "will"! :-)
Thanks for the tip. Please use a radiused end mill Ken.

According to Roark Formulas for Stress and Strain.
The max stress on a solid rectangular beam six inches high by 1/2
inch thick with a 200 pound cantilever load eight inches out
is is M * c / I  

c = 3 inches half the height of the beam
M = 1600 inch pounds bending moment. 8" X 200 #

and I = 1/12 X (b * d^3)

b = .5 the width
d = 6  the height  
d^3 = 216

so I = 9 moment of inertia

max stress = (1600 X 3) / 9 or about 500 psi tensile.
6061 T6 will easily take 40,000 psi on a bad day so this is 
not just over kill! It is 80 times stronger than it need be for
the static load. For a six G drop with 1000 pounds on
the end it is 2,700 psi tensile or 15 times stronger 
than it need be.

I really don't think we need to worry about fatigue here.
Not unless you plan to drop it in a million times.

Paul Lamar
 
The AirCraft Rotary Engine NewsLetter.              Powered by Linux.
ACRE NL web site.
http://home.earthlink.net/~rotaryeng/            http://www.linux.org