Monty Roberts wrote:
Most of this has been tried including Nickasil. None of it works
as well as detonation gun application. The particles travel
at near supersonic speed and imbed themselves in the aluminum.
What has not been tried to my knowledge is a two piece end housing
like this. This can be made on an ordinary NC mill out of billet aluminum.
The water passages of the stock end housing must be duplicated.
Paul Lamar
Paul,
This would work great (I think). I have an NC mill that I am rebuilding that
could handle a part this size. Might be worth a try for a ground based
engine trial. Every single engine I have has bad end housings. I might as
well try it. I could build the end housings for less than the cost of buying
new iron ones. I can cut open the ones I have and digitize the water
passages etc. Thermal expansion will have to be considered I imagine. I
wonder if there would be a problem with the thin steel metal peice warping.
Oh well, time to try it and see.
One other thing that I have considered is to use explosive welding to add a
thin coating of hard steel to a cast aluminum housing. then lapping it flat
in the typical manner. Not sure if you would have problems with the steel
being too brittle. You might be able to get away with using something
relatively ductile, and then using the nitriding process to harden the
steel. Not sure what this would do to the aluminum though. This is used in
aerospace and also naval applications. You can join an aluminum
superstructure to a steel hull in this manner.
For more info see:
http://www.wsu.edu/~jeffhall/me310/exp.html
I had wondered about flame and plasma spraying. I have a freind who does
this kind of thing for aerospace parts, but guess it hasn't worked in the
past. My wife is a mechanical engineer who designs aluminum wheels for the
auto industry, so I have a great consultant (and relatively inexpensive
too!!) when it comes to low pressure aluminum casting design.
Monty
The beauty of the separate steel wear piece is they can be laser cut mass produced
and sold as low cost replacements. You can control the hardness better too.
Or porous chrome plate them if you wish. My guess is 3/16 ought to be a good
starting thickness. Thicker if they warp. The back housing is the heaviest
and would be a good trial.
BTW chrome don't stick to aluminum too good. Especially when heat is involved.
In case somebody was wondering why we did not just chrome plate an aluminum
casting.
Paul Lamar
The AirCraft Rotary Engine NewsLetter. Powered by Linux.
ACRE NL web site.
http://home.earthlink.net/~rotaryeng/ http://www.linux.org