Subject: 2 rotor Turbo Manifolds
From: ACRE NL
Date: 3/7/2002, 11:59 AM


Here is the two rotor version.

Paul Lamar

  That's a nice piece of work but obviously not the $600 cast iron
piece
that Chrissi was talking about. What's the cost on this one? And
what ss
alloy? Wall thickness? Are you sure you have that weight right? Cant
see
how the flange alone would be that light let alone the entire
manifold
unless its paper thin material.

Mike Wills


There was evidence that they did not know how to weld stainless tube.
There was inside flash on the welds and that is a sure sign helium
or argon purge was not used inside the tubing. This is recommended
when welding SS tubing. You would have to go in with a die grinder
and clean up the inside of the welds.

Also I question the durability when compared to a heavy cast iron
turbo exhaust manifold.

Now here is a nice one made from Inconel that cost Jim Mederer $3000.
Its got a couple of hundred hours at the 900 HP level so far.


Paul's remarks are about the 3 rotor ss turbo exhaust. I believe it will
be sufficient as will be inspected often. I will also probably coat it
with one of the high temp 2000 degree coatings as well-they have to
clean up the insides and edges before coating (Jet Hot did this with
this custom heavy gauge steel 2 rotor turbo manifold you see pictured
here [with 2000 F coating on inside and outside], done for me in
Florida. Steel weighs not much more than the ss one at 13 Lbs, 10 oz!!
including the inside and outside coatings. )
I gave bum info on the HKS ss 2 rotor unit, I quoted the weight of the
external aircraft type wastegate flapper valve instead of the manifold
(what was I thinking?)
The 2 rotor is HKS, I believe you can find the specs on the web. I
believe the alloy is 304 ss. All welds in the 2 rotor are smooth inside.
Rechecking the weight, it is 10 lbs 7 oz (about 3 lbs less than heavy
gauge steel). It is extremely well made and has no rough inside edges or
flash at all. Looks like it has been ground inside!
Tough to assess the gauge of metal of the ss pipes. As I have have to
drill/weld for the EGT and TIT weld-o-lets (when I get around to it) I
can check it then.
If I could weld like any of these, I would have made my own and included
those fancy bellows expansion pieces (which you can get in 2 ply .016
304 ss from JC Whitney, as well as Burns!)

[Marc Wiese]

Racing Beat used Inconel bellows.
Thick mild steel is the way to go. Ceramic coating will delay the
flaking corrosion.

Paul Lamar

 
The AirCraft Rotary Engine NewsLetter.              Powered by Linux.
ACRE NL web site.
http://home.earthlink.net/~rotaryeng/            http://www.linux.org

HKS_ss_2_rotor-weld_details.JPG

2_rotor_steel_manifold-B.JPG

2_rotor_steel_manifold.JPG