"F. J. Diekman" wrote:

The limitations of shot peening as far as threads go are the size of the
shot.  Smaller shot = thinner layer of compressive residual stress, and
lower values of stress.  Obviously you can not use a large shot size and
expect to get down into the root of the thread.  But using a very fine shot
size followed up with some fine glass beads will give you compressive
stresses in that area, and the double peening will give you extended fatigue
life.  If you are worried about surface finish, again, the combination of
the small steel shot and the glass beads will give you a surface finish that
is acceptable.  I have shot peened a lot of different items, including screw
threads when I owned a shot peening company, and it is a very under used
process for the benefits that can be had.


These bolts are like 5/16 24 or 8 mm metric equivalent.
That is real fine shot indeed.

Paul Lamar


Paul, If strength of the tension bolt threads is a problem why wouldn't a standard "j" rolled thread form, followed by shot peening the shank handle the problem?
Bill Jepson

It might but I think it is the wrong approach. Better to change the resonant frequency
or stop it from vibrating somehow. The bolts are plenty strong for the purpose.

Paul Lamar
 
The AirCraft Rotary Engine NewsLetter.              Powered by Linux.
ACRE NL web site. Copyright 1998-2002 All world wide rights reserved.
http://home.earthlink.net/~rotaryeng/            http://www.linux.org