> > > > EGT's run 1400 to 1700 degrees F. What we have found to work
well is
> > > to just compromise on the weight a bit and go to thicker wall
stainless tubing.
snips....
Jack Dougherty wrote:
Paul,
I've been told by a freind, who has been a welding supervisor in
refineries
for many years, that 4130 will stand the heat much better than any
stainless. If the heat is too much for that he says you need inconel or
monel, but for the temp we would see on exhaust, he thinks rust may
be the
only downside. It certainly would be much cheaper to construct.
What do you think...............Jack
Jack,
After reading this, I plunked a piece of 4130 into the forge. The
result is that it flakes much less than mild steel but it still
flakes. The flaking appearance is very different, the 4130 flakes
are very tiny, like pits. I don't think it would last long enough
to justify consideration. . The other comment I would like to make
is about expense. Two points: considering labor, I would opt for
the exhuast material that promised the longest life. This seems to
be a relatively thick wall SS. However, .065 is not that thick and
not that heavy. The second point is to shop around for the SS
tubing. Stainless Steel Specialities was ten times , let me say that
again, TEN TIMES less expensive than Tube Supply on identical pieces.
Jerry
-Mark Steitle wrote:
Jerry,
Can you provide contact information on Stainless Steel Specialties?
Thanks,
Mark