Subject: 304 heat resistance
From: ACRE
Date: 3/18/2003, 11:49 PM

Jerry Hey wrote:

I placed a piece of .032 304 SS in my forge directly under the blast.
The forge bottom  is eroded from  years of exposure to the blast  so
there is a low spot.  The test piece of 304 bridged this low area so
that the hot spot  area was not supported or cooled by contact.    I
ran the forge at low pressure for about ten minutes holding the heat
down to bright red.  I could not see any effect on the test piece.
Then I turned the pressure up.    Within seconds the test piece became
bright orange, but not white. The  photo is a little brighter than the
reality.   After twenty minutes at this temp, the sample began to flake
and I stopped the test.  While I intend to test longer at lower temps,
I think it is safe to say that if  you run your engine at night and
observe the exhaust pipes, if  you see a color that is even suggestive
of orange, you can expect 304 to fail eventually.  On the other hand,
if the color is any phase of red including bright red,  then 304 may
hold up. I will run a longer  test at bright red in a few days.    I
have not done a cone test on the forge in years but bright orange
should be around 1700.  If anyone has a heat/color chart they can check
me on this.   I want to point out that the inside of my forge is a
worst case scenero.  It is designed to focus heat and get metal  HOT.
   If the 304 piece was exposed  to cooling air such as the outside of
an exhaust pipe, it would be difficult to heat to orange, I think.

So, what exhaust temps does the rotary produce?   Jerry

Up to 1800 F.

Paul Lamar
 