How hard does the steel plate have to be hardened to achieve the
same
wear
characteristics as the stock housings, and Racing Beats aluminum
housings?
Royce
My guess is around Rockwell C60. I don't know what RB uses for
coatings.
I don't think it will ever be as hard as tungsten carbide but then
there is no possibility of it flaking off either.
Paul Lamar
Paul,
Great !! but I'm a little confused.
Do you intend to use a carbon type steel and heat treat it through
to
Rockwell C 60 or a mild steel with a surface treatment.
George (down under).
Carbon chrome molly steel. 4130 or 4340. Heat treated.
Paul Lamar
We have cut about 6 engines into iddy biddy pieces to see how it is
made, how it
works, and how it can be hot rodded.
In doing all this we decided to abandon the idea of mixing two different
metals
for several reasons.
We now know how to mill two aluminum plates that get bolted together to
form
each housing.
No wear plate needed, and no problems of seperation or flaking.
Anyone with a "cc" mill and aluminum drops can make their own end
housings.
It's a simple process.
Royce
Mark wrote:
Hi Royce, do you have any photo's of housing you have made like this. How
many hours, miles has your highest time component. Have you pulled an engine
down and done a condition inspection of a used housing. Pictures?