Carbon chrome molly steel. 4130 or 4340. Heat treated.
Paul Lamar
We have cut about 6 engines into iddy biddy pieces to see how it is
made, how it
works, and how it can be hot rodded.
In doing all this we decided to abandon the idea of mixing two different
metals
for several reasons.
We now know how to mill two aluminum plates that get bolted together to
form
each housing.
No wear plate needed, and no problems of seperation or flaking.
Anyone with a "cc" mill and aluminum drops can make their own end
housings.
It's a simple process.
Royce
Royce,
How do you propose sealing the "two aluminium panels", from my observations
(cut housings) there is little room for simple O-ring seals. The bolts also
need to be sealed and there is the inlet areas which are difficult. I assume
the water jacket area can be reduced to address those problems - is this
what you propose.
Also what do you propose for a wear surface.
Paul,
I'm still concerned with using a carbon material like chrome molly -
although it's bloody good stuff.
There a whole heap of heat issues which can and will affect it and I don't
know if that will significantly affect the wear surface - I assume it will
!!
George (down under)
My foundry guy does not think so. Since the side housing temp rarely
exceeds 250 F we are not worried. Also Mazda does the same thing
on the rotor housings. If you look closely you will see a thin
steel insert in the rotor housing casting that is then chrome plated.
Chrome plating over the steel insert is one of our options.
Chrome plating over aluminum is known to cause problems.
Paul Lamar