Also I have heard rumors that Midwest also had problems
with nicka-sil.
My inclination is to go with something that is known to work and
that is hard ferrous metals. My foundry has extensive
experience
with embedding ferrous metals in aluminum castings.
That minimizes the long term risk.
Paul Lamar
Paul, Kawasaki had enough trouble with Nickasil bores that they developed a completely different process for their 2 strokes. I mentioned the electrofusion process in a previous post. The advantage is that the material bonds at the molelecular level. LA Sleeve still does Nickasil plating for AL bores. Flaking is always a possible problem, with disasterous results. I haven't been able to access the carrocos web site for the SAE paper you mentioned. Just kicks you out. One of the guys here where I work wants to see if we could duplicate the process but I need a reference. Any sources besides the SAE Mazda paper? Bill Jepson
Not that I know of. I don't know what is going on with Todd Carrico as his email
is now bouncing.
Paul Lamar