Ed Anderson wrote:
Hi Paul,
As you know, the BurnsStainless bent aluminum tubing is annealed to "O"
condition before bending - leaving it somewhat softer than desired for our
applications. See extract below, it appears that by sticking it into a
regular electric (not microwave) and baking it for 8 hours you can get it
back to T-6 condition. (hate to think what the electicity cost would be).
I think I may try that with my intake manifold just to see.
Ed Anderson
Jim Millett, president of U.S. Light Aircraft Corp., told us something that
illustrates the peculiarities one can encounter in the field of heat
treating aluminum. He suggests taking a small piece of 6061-T6 sheet and
trying to bend it with your hands. You will find it to be very strong and
springy. Then heat it to 950 degrees. This could be done in a pottery kiln
or by using a propane torch to heat it evenly until the surface turns gray.
Then immerse it in cold water. This is what is called "solution heat
treatment." The sample is now in the 6061-0 condition, the last "0" meaning
that it has been annealed to dead soft and easily bent condition. Then bake
it in a kitchen oven at 350 degrees for eight hours. This is called
"precipitation hardening" and the sample is now back to the 6061-T6
condition and just as strong as it originally was.
Ed Anderson
Matthews, NC
RV-6A N494BW
eanderson@carolina.rr.com
Funny you should mention that now. I am about to pick up about 120 bends from the
bender and take them over to the heat treater.
How does it feel in the O condition. Can you easily bend or dent the .058 scrap?
BTW the legs on those bends look very long. What did Burns charge
you for those bends? I assume you are going to cut them off around
17 inches.
Paul Lamar