Subject: An Extra E
From: ACRE
Date: 2/5/2004, 10:39 AM


George Lendich wrote:


    Did you see Don Dunbar's statement on welding sand castings
    - can be
difficult because of the silicone (sand) contaminating the surface.
A good heads-up IMOP.

George (down under)

Jack Beale wrote:

George,


    After reading so many messages, I just gotta tell 'ya:
S-I-L-I-C-O-N-E... is used to make titties bigger.  S-I-L-I-C-O-N is
the sand you refer to, and what they make computer chips outta...

    I believe that the sand (that's used in the mold) gets into
    surface
of the finished piece and causes both welding and machining
problems.

Jack Beale
jack.beale@att.net

Gee Jack - I know the difference, a bit of a typo, what's an E or
two between friends.

 I tell you this as I'm Just likely to do it again sometime, like
 the advert
goes - " I don't know how I can live with myself !?'
George (down under)

George,

You need to ask Dan Quayle what an extra E can do for ya!

(In case you Aussies don't follow US politics too closely, he had a
little trouble spelling potato during a campaing a few years back.)

Bob White

- - - - - - -
http://www.bob-white.com
N93BD - Rotary Powered BD-4

 
The AirCraft Rotary Engine NewsLetter.  Powered by Linux.
ACRE NL web site. http://home.earthlink.net/~rotaryeng/            
Copyright 1998-2003 All world wide rights reserved.