> Russell,
> Hydrogen embrittlement is more of a problem
> on steel parts than aluminum. The problem on
> Al is making it stick!
> Bill Jepson
Maybe they were merely polished.
Paul Lamar
Paul, they were probably chromed. It is easily done
with a 3 layer system. Copper first, then nickel, and
then chrome. Just costs more. Must be polished twice
as well if your copper plate isn't perfect.
Bill Jepson