Paul,
Will the bond hold with the heat cycling?

Paul Lamar responded:

Sure. The end housing run a maximum of 500 degrees  F worst case.
Probably more like 350 degrees F. If differential expansion was a real
problem we would have problems with the stock steel liners in the aluminum
rotor housings. They do indeed run at 500 F or more.

Can the Cte problems be mitigated by deta-coupling the metals at an elevated
temperature?  I'm proposing heating the metals to 200-300 degF then deta-coupling
them.

Russell Kent

Don't know Russell. We should contact:

Joe Graham wrote:
 Several months ago I spoke with Jose Olivas of Dynamic Materials Corp.,
(used to be Explosive Fabricators, I believe), They have an office near
Boulder, CO. His Ph No. is 1-303-604-3910, and e-mail at
jolivas@dynamicmaterials.com. 

and ask some questions. What strikes me about this (sorry about the pun :))
is the similarity with detonations coatings that also work very well.
In this case a whole sheet of material is blasted instead of only
small particles.

BTW are you guys not getting this email lately?

Paul Lamar
 
The AirCraft Rotary Engine NewsLetter.  Powered by Linux.
ACRE NL web site. http://home.earthlink.net/~rotaryeng/            
Copyright 1998-2003 All world wide rights reserved.