I would want at least an 1/8 inch to give some room for surfacing
> and resurfacing in the future and to give a more rigid plate to
deal
> with warpage.
> It may be more cost effective to buy a thicker piece they have
in
> stock and CNC mill it out and if the surface is to soft hard
chrome
> or cermachrome plate it.
>
> Ken
Ken, I understand the desire for a thicker steel plate to allow a
"fudge factor" when machining. But the chrome plating mystifies
me. Why not nitride the surface as is done on the standard Mazda
plates? This is a simple reliable treatment, that is a molecular level
physical change and doesn't flake off like most chrome treatments can.
Bill Jepson
Bill,
I must say, after considerable thought over many months, my thoughts are in
line with your own on surface finishes.
George (down under)
The AirCraft Rotary Engine NewsLetter. Powered by Linux.