Ken, I will have to withdraw my comment about the chrome surfacing.
Since the idea was to apply the steel cladding to a aluminum sheet and then
furnace braze
the part to an end housing nitriding might be too hot a process for the
binding material used in the AL braze process. (Gas Nitride is usually done
at about
900°F) The fact is that the aluminum will nitride as well which might
make it brittle.
Bill Jepson

Archie wrote:

Just a comment while on this subject.
We made several sets of lightweight titanium wristpins for testing
on endurance type V-8 racing engines.
They were gas ion nitrided, and run with no problems for many
races. Upon disassembly, no apparent problems, and were
re-used again. At this point, not sure if the cost of fabrication
is justified, however.
Archie 