Brian Trubee wrote:
This is a bit off topic, but I was wondering how aluminum is
tempered or conditioned. I've got a bunch of .063 2024 T0, but
I need some 2024 T3. Is there some practical way at home that
I can treat the 2024 to bring it to a T3 condition? Anyone?
Brian,
If the 2024-T0 has sat around for a while, it most likely is no longer
T0.
This website indicates that 2024-T0 will naturally age and harden to T3
over the course of *4* days (wow!). You might want to do a more
thorough research than I did, however.
http://www.key-to-metals.com/PrintArticle.asp?ID=39
Russell Kent