> I 've been thinking about using the Schedule 40 304 stainless for the first foot or so of my exhaust system, but I can't bends that tight -2" inside diameter with 2.35 OD pipe. What I
have now is
> 2"Diameter .049 321 Stainless bends. I'm a little concerned that the bending stretched the material to an unacceptable thinness right where the pipes are the hottest.
> Of course I am going to have a SS heat shield completely surrounding my exhaust system, but I was wondering if ceramic coating the pipes would help keep the pipes intact.
>
> Anyone?
>
> Brian Trubee
I think you would be better off welding a conformable patch on the pipe.
Ed Anderson 304 SS .140 wall exhaust pipes don't even discolor :)
Paul Lamar
I have thought about a conformable patch, my concern there is that perhaps the weld bead itself would be a stress point. I use a TIG welder with the appropriate rod for the material, so maybe I'm
worrying too much, if that is possible.
Brian Trubee
The Rotary Engine NewsLetter. Powered by Linux.