<< I 've been thinking about using the Schedule 40 304 stainless for the
first foot or so of my exhaust system, but I can't bends that tight -2" inside
diameter with 2.35 OD pipe. What I have
> now is
> > 2"Diameter .049 321 Stainless bends. I'm a little concerned that
the bending stretched the material to an unacceptable thinness right where the
pipes are the hottest.
> > Of course I am going to have a SS heat shield completely
surrounding my exhaust system, but I was wondering if ceramic coating the pipes would
help keep the pipes intact.
> >
> > Anyone?
> >
> > Brian Trubee
>>
I used .120" wall mild steel tubing for primaty headers. I wrapped them with
heat tape. three weekends after I added the heat tape I notices a clump of the
tape missing. I crushed the tube with my hand. It was like thinwall glass.
Then the tube bender made up son 90s for me from .140" wall stuff he had on
hand.
I did not wrap them and have a blast tube blowing on them no problem in 6
years.
Thick wall stainless sounds real good to me.
Lynn E. Hanover
Mild steel exfoliates.