Subject: Aluminium end housings
From: Rotary Engine
Date: 3/30/2006, 5:03 PM
To: AAme



    Electrochemical metallizing is a technological br-
    eakthrough, an improvement over a process originally termed "brush
    plating". Thin (0.0001 in. to 0.01 in.) metallic coatings are
    applied at
    low temperature.

    One thou (.001) is not very thick.


Hi Paul,
0.01" is ten thou. How thick do you think we need on the end housings?
And, tell me again why the same process that is used to give the rotor
housing its steel liner cannot be used on the end housing. I know we
have 'done it to death' in the past, but my old brain drops info like
confetti these days!
BR, Dave McC (still building the Europa; it never ends)

Ops. Read it wrong. I see no reason why that can't be done.
If there were 10 of me I might get around to getting
my NC mill working, make a pattern for casting end housings and
have some cast up with steel liners like Mazda does it.
My foundry says no problem casting steel inserts.

I have to set priorities. It think a BSFC of .375 is more important
right at the moment.


Paul Lamar ...No rotor no motor.

The Rotary Engine NewsLetter. Powered by Linux.
ACRE NL web site. http://www.rotaryeng.net