Subject: Aluminum center/end plate ?
From: Rotary Engine
Date: 2/22/2007, 3:15 PM
To: AARotary Engine

    >
    >  > Paul: You, any one else, ever look at RB's aluminum end and center
    > housings
    >  > and wonder how much trouble to machine out of solid aluminum
   billets
    > for
    >  > PPort engines? After all, they won't need intake ports in them.
    >  > jofarr, soddy tn
    >  >
    >  > Can't be done because they are hollow. Now if somebody invented
    >  > a tiny robot milling machine that you could put down a small hole
    >  > and have it mine out cavities in the material that would work.
    >  >
    >  > No intake ports would certainly help.
    >  >
    >  > If you made them in two pieces that would also work if you could
    >  > figure out a way to seal the internal joints. Could be done with
    >  > some sort of gasket or O-rings and that is exactly what Richard
    >  > Sohn is working on.
    >  >
    >  > Paul Lamar ...No rotor no motor.
    >  >
    >  > Paul,
    >  > Those two pieces could easily be furnace brazed together.
   According to
    >  > Alan Tolle Everett even did a steel 2 piece milled and furnace
   brazed.
    >  > For the "superlite" engine. For aluminum the problem remains the
    > coating.
    >  > I'm convinced that it would be "do able" just expensive. I
   think that
    > the
    >  > state of milling equipment probably do a better and faster job
   than
    >  > casting.
    >  > Bill Jepson
    >
    >  > hi Bill, this is the way my machinist and i have planned to do
   it. what
    >  > would you estimate the cost of casting them? just so i could
   compare
    > costs.
    >  >thanks , wyo. walt.
    >
    > Walt
    > The problem is the cost of the pattern making. You could easily
   spend 10K
    >  to 15K setting up the patterns to cast the various parts. That
   is before
    > making a single casting. Additionally the sad thing is you could find
    > that your
    > casting still didn't work due to porosity or core shift. The fact is
    > that billet
    > construction would probably be cheaper until at least the 100
   unit mark.
    > machining from billet you have a reasonable expectation that your
   first
    > part
    > would work. All the aluminum concerns about coating are about the
   same.
    > Bill Jepson
    >
    > One possible problem I can see Bill is the compressive strength
    > of furnace braze is not as high as the base material.
    > The tension bolts put a lot of compressive stress on
    > the engine end housings.
    >
    > Paul Lamar
    >
    > Paul,
    > This is a reasonable concern, but with proper layout shouldn't be a
    > problem
    > The key is to place the braze material around the piers or in a
   center
    > reservoir
    > so the base material is in near contact. (a super thin film is
   wicked to
    > the base
    > material by heat and usually a flux) The way I've seen this done
   is to
    > weight
    > the two parts together to force out excess. Your separate wear
   surface
    > idea
    > with o-ring seals is another way to do this. (I thought that hot
   rivets
    > from
    > opposite sides could hold the plates in place) Lastly, modern
   thermally
    > conductive epoxies could be used to fasten interlocking opposite
   sides.
    > For
    > the CNC milled parts that might be the most effective method of
   all. the
    > parts could be well located and pressed together during cure. Detgun
    > coating
    > for least unwanted heat transfer. There are many ways to go after
   this, I
    > wish I had the money to pursue it. FWIW
    >
    > Bill Jepson
    >
    > JB Weld them together might work.
    >
    > Paul Lamar
    >
    > Paul,
    >  If you setup the edges that come together like this, with a small
    > clearance
    >  to allow the epoxy somewhere to go, it would work fine. You
   could do the
    > brazed part exactly the same way, only the clearances would change.
    > Pardon the crude model but the concept is obvious.
    > Bill Jepson
    >
    > That jpg did not work.
    >
    > Paul Lamar

   Paul,
   With the differential thermal expansion of the center plate,( two
   combustion
   chambers and cooling water between), it appears that there could be
   tension
   in any internal ribs passing from one face to the other. Any joining
   method
   would have to accommodate this.

   Colin Smith

   Possibly. Short of an FEA we would not know for sure.
   Do you have an FEA available?

   Paul Lamar ...No rotor no motor.


Does the aluminum piece have to be done in halves?

Can an iron/steel wear surface used which also bridges the openings in
the housing which allow for the machining to be done?

A one piece housing might be fairly crudely cast.  Then put it through a
finish milling process to touch things up where precise tolerances are
required.  Mill where the iron wear surface fits plus an o-ring groove
to seal it.  Might be cheaper overall than taking huge billets of Al and
milling them out.  And you might get away without gluing anything together.


Matt-



The Rotary Engine NewsLetter. Powered by Linux.
ACRE NL web site. http://www.rotaryeng.net
Copyright 1998-2006 All world wide rights reserved.