SS is readily brazed using high or low temperature brazes or
solders. Pure copper can be used as a brazing material at 2050 -
2100 F with a hydrogen atmosphere without a flux. Silver and silver
alloys used for brazing are used at a much lower temp but usually
require a flux. Brazed surfaces must be very clean for a good
braze. Joint gap thicknesses of 0.001" - 0.003 " are optimum for
high strength. An acetylene flame can be used for the heat source.
Joel
Over the Hill Materials Engr.
I don't think we want to hit the inside of the rotor housing
with an acetylene flame.
Paul Lamar
Hi Joel,
Perhaps you meant with a 'nitrogen' atmosphere?
Rolf
The Rotary Engine NewsLetter. Powered by Linux.