I just had an idea that will take a lot of the technical risk
out of welding in SS P-port tubes.
The procedure is; remove the aluminum back about 1/4 inch all the way
around
the inside of the water jacket next to the steel liner. See the photos.
This will cut down on the tig welding heat required to weld in the SS tube
to the steel liner. Normally a lot of welding heat would be conducted away
by
this aluminum or worse melt the aluminum. This aluminum will be replaced
by JB Weld when finally potted. The unsupported steel liner is not
a problem in this area in this area of the rotor housing as pressure
is very low to near zero.
This is a peice of cake if done on a mill using a special cutter mounted
in a boring head holding an ordinary 1/4 inch lathe tool bit. See the 3Ds
and picts.
Some clean up will be required using a die grinder.
It can also be done by hand with a die grinder.
For those new people on the list P-ports are good for 40 to 50 HP
more at 6500 to 7500 RPM range.
Paul Lamar ...No rotor no motor.
Paul,
Good thinking, I was a little concerned about the aluminum but thought a
wet rag might do the trick, but your right, it will suck down the heat.
Another way would be to cut the hole 1'4" bigger right up to the steel liner
(all the way through the aluminum) and slip a collar on the tube, maybe
pre-weld it to the tube.
Or weld in an aluminum collar to the outer side of the housing with an O
ring groove you could then side the steel tube into position through the O
ring and weld to the liner. Still have to use wet rags as the heat travels
through that SS quickly. There would be no leaks that way and you might not
need to fill the void. A couple of things to consider over and above that,
but perhaps another alternative.
Just some thoughts!
George ( down under)