Subject: Welded in P-port tubes
From: Rotary Engine
Date: 6/14/2007, 8:09 AM
To: AARotary Engine




Paul, Is there any effect on the metallurgy of the liner due to the heating
during the welding process that could adversely affect the apex seal sealing
and or wear?
Joe Berki Limo EZ
I can't detect any. The apex seals cannot seal in this area as they are wide open on both sides as they pass over the intake port. That is why the differential pressure from chamber to chamber is zero in this area. Tig welding is a very localized heating process. Obviously the steel must be heated to melting temperature but a few hundreds of an inch away the aluminum is not melted.
This process flies in the face of intuition. The metal has a worse time of it down by the peripheral exhaust ports where the heat can be 1800 F for thousands of hours.
Paul Lamar ...No rotor no motor.

Paul,
I do question the fact that the welding process causes the inclusion
of chromimum. The hard chrome process which coats the liner will be
fused into the weld. This could cause a brittle weld. There may not be
enough inclusion to be a big factor but very small amounts can change
the metalurgy. I'm not chemically astute enough to tell you how much
might be needed to cause a problem.
Bill Jepson
Yes it changes the 304 Stainless Steel or mild steel to chrome molly :)
If you start with 4130 tubes you get chrome chrome molly :)

What do you get when you weld mild steel to SS?

Answer: No problems:)

What do you get when you weld mild steel to 4130?

Answer: No problems:)

There is near zero load on the tube and it never gets over 200 F
if that.

We are not talking about stressing the part to 65,000 psi.
It will be lucky to see 600 psi.

Paul Lamar ...No rotor no motor.