Paul,
Is there any effect on the metallurgy of the liner due to the heating
during
the welding process that could adversely affect the apex seal sealing
and or
wear?
Joe Berki
Limo EZ
I can't detect any. The apex seals cannot seal in this area as they
are wide open on both sides as they pass over the intake port.
That is why the differential pressure from chamber to chamber is
zero in this area. Tig welding is a very localized heating process.
Obviously the steel must be heated to melting temperature but
a few hundreds of an inch away the aluminum is not melted.
This process flies in the face of intuition. The metal has a
worse time of it down by the peripheral exhaust ports where
the heat can be 1800 F for thousands of hours.
Paul Lamar ...No rotor no motor.
Paul,
I do question the fact that the welding process causes the inclusion
of chromimum. The hard chrome process which coats the liner will be
fused into the weld. This could cause a brittle weld. There may not be
enough inclusion to be a big factor but very small amounts can change
the metalurgy. I'm not chemically astute enough to tell you how much
might be needed to cause a problem.
Bill Jepson
Yes it changes the 304 Stainless Steel or mild steel to chrome molly :)
If you start with 4130 tubes you get chrome chrome molly :)
What do you get when you weld mild steel to SS?
Answer: No problems:)
What do you get when you weld mild steel to 4130?
Answer: No problems:)
There is near zero load on the tube and it never gets over 200 F
if that.
We are not talking about stressing the part to 65,000 psi.
It will be lucky to see 600 psi.
Paul Lamar ...No rotor no motor.
Bill, Paul
What is the largest P-port across you have seen? Here is the challenge as I
see it. If you want a Leman style 2 inch ID port then that is 50.8mm (close
to 51mm)
If the SUS 304 pipe goes all of the way through and has a wall thickness of
1.5mm or 0.06" then that will bring the outer edge of the insert to 54mm in
diameter. Assuming an expert weld in the widest part of insert then about 1
mm on each side of the insert will be added. This welded area will be
harder then the rotary housing wall because of chrome migration during
welding. Buffing the weld out it will widen the port even more. Softer
metal sands faster. OK you have a super technican perform the operation and
mask carefully. Still it is conceivable that the widest unsupported seal
area will be about 57 to 58mm wide. That leaves 11mm on each side to
support the seal in that area. Is this enough?
Doug
Well first we are using 2 inch OD .065 wall (but I am thinking I will
use .049 wall on the RX8 engine) 2 inches is 50.8 mm The housings is 80 mm or about
14.6 mm each side to support the apex seal.
The peripheral exhaust port used in the millions
for 35 years or more has about .7 inches or 17 mm on either side.
So far 14.6 mm seems to be enough but make it less at your own risk.
I am thinking of using 2 inch ID 2-1/8 OD tubing but only beyond the
slide throttle. I will then have a slight venturi effect for
the mechanical fuel injection.
--
Paul Lamar ...No rotor no motor.