Subject: Higher power for your rotary. Maybe a breakthrough???
From: Rotary Engine
Date: 6/19/2008, 10:57 PM
To: AAA Put this in the To box


    > Paul,
    > If the new corner seals use DLC, having a nitrided or other hard
    > material on the side plates becomes very important. Any idea if they
    > used those corner seals on the LeMans engine?
    > Bill Jepson

   Bill,
   Everything I have been told about mating wearing surfaces tells me the
   hardest surface wins the wear war. However Larry did say "hard and
   slippery", perhaps the slipperiness of the material may off-set the
   tendency
   for higher wear of the side housings.

   Then again why is it so slippery - I can only imagine that it is
   somewhat
   porous and holds an oil film.

   The small contact area of the corner seal, is the main side housing wear
   evidenced in most engines in the past and is the main stumbling
   block to the
   successful development of the aluminum side housings IMHO.
   Perhaps then, this development has helped overcome that particular wear
   problem - but I'm only guessing.
   George (down under)

George,
The definition of "wear" and the definition of "hard" are two of the
most relative terms in engineering IMO. To have good wear you need two
levels of hardness even when lubricated. Usually the softer of the two
materials is expected to slough off material. The rate at which it does
that is the critical thing obviously. For instance the ceramic apex
seals are harder than the chrome surface of the inner rotor housing
face. The chrome is hard enough though that the rate of wear on the
housing is very slow. Getting two materials that are just far enough
apart on the hardness scale is the crucial point. Raw cast iron wouldn't
be good there. The nitride coating put on the standard side plates is
very thin but quite hard.
Bill Jepson