Started all over.
Ground off all of the JB weld outside
Ground off the JB weld inside around the bolt penetrations
Drilled and tapped for 1/4-28
Drilled sealplate for 1/4" bolts
Wrapped sealplae in packing tape
Alodined the aluminum using aluminum prep from auto body supplier
It actually was a golden brown after the alodine was applied and rinsed
Applied JB weld outside all around the SS tube in the area previously
alodined.
Applied vasoline to the threaded surfaces
Mounted sealplate and torqued fasteners
Wiped excess JB weld off of housing
Let cure
-----------------------------------------------
Phase 2
Removed 1/4" bolts and cleaned threads with lacquer thinner
Removed sealplate
Cleaned and alodined
Cleaned threaded holes and cavities below with lacquer thinner
Loaded the surface up with red RTV
Installed new O ring in sealplate
Mounted sealplate
Coated threads on bolts with red RTV and installed
Torqued bolts and cleaned off excess RTV
Joe Berki
Limo EZ
--