This was a wild ass guess on current (80
amps), gas flow
(12.5 CFH) and tungsten
distance (about 1/8 inch).
The 60 Cycle synchronous gear motor was rotating at 1
RPM.
You can set your watch on it.
I am going to have a party tonight :)
This is as close to a perfect weld as it gets.
The last picture was some welding done by the best
welder I
know. He is a guy that works for
George Talbot Talins company in Torrance Ca.
Paul Lamar
That looks very good. Is that autogeneous welding or
are you
using filler?
You might make the taper a tad longer on the electrode.
Typicly 2 to 1-1/2
electrode diameter. What is the make/model of your welder
power source?
C. Smith
Thanks for the tip (pun unintended) :)
I'll try that.
Do you know of a hand held device that one can put a
length
of tungsten electrode in and have it rotate it while you
are grinding the tip? In theory the tip would come out
perfectly
symmetrical.
What is autogeneous welding ?
No filler rod.
Lincoln square wave tig 175 pro.
Paul Lamar
Just one other note. I see in the image you have the
grounding wires looped
around the workpiece. In general this is not recommended
practice, because
you have effectively created an iron core inductor. This
will resist the
flow of current (causing you to use a setting higher than
necessary), it
also will add to the heat in your ground circuit. When you
get into
"production" this may lead to your ground wires getting hot.
Avoid loops in
welding circuits.
C. Smith
It has had no affect I can detect so far.
Still one long line.
BTW I got the money for the oil pan. Thanks.
If some of you have not sent in your deposit for the oil pan
on this go
around the price will go up.
Paul Lamar
I just thought about it again, you are welding carbon
steel, DC welding. No inductive effects. I'm used to AC
welding currents in resistance welding and aluminum. Sorry.
C. Smith
The Rotary Engine News Letter. Powered by Linux.