Hi Paul. I am revisiting the long drive shaft for a pusher design.
With the progress made on composite drive shaft, is the option of
long and light prop shaft becoming more of a reality now? I saw a
lot of automotive carbon shafts on the market now for very decent
prices. Could a simpler design with rubber couplings instead of
power/slip clutch be made to work without outlandish development cost
and headache? I would appreciate your thought. Luke F Wings.
How long?
I would use a minimum of 3.5 inch diameter aluminum tube. Cut the
wall thickness on a lathe to .062" to save weight. Then anodize it
so epoxy will stick . diagonally wrap carbon fiber to a total
thickness of .125 to .2 inch.
If not too long get a stock RX8 carbon drive shaft from a junk
yard. Yes rubber couplings are the way to go.
Paul Lamar
Will anodizing be as good as the process used on grumman GA? THANKS.
L F WINGS.
I don't know what they used on that airplane. You can buy a kit in
West Marine to treat aluminum for epoxy bonding.
How long is the prop shaft?
Paul Lamar
Isn't there a vibration issue with anodized parts. There was an award
winning Experimental helicopter where the builder had anodized a lot of
parts for a blingier look, including I think the drive shaft. After about 60
hours the blingy part failed catastrophically causing a complete wreck
of the
machine. IIRC the anodizing process introduces microscopic stress risers.
Feel free to correct me if I've got this all buggered up.
John Gibbons
The aluminum tube is just a male mold for the carbon fiber.
BTW when you have a high modules of elasticity material (carbon) sharing
the load
with a low modulus of elasticity material (aluminum) the high modules
material takes
most of the load.
Paul Lamar