I came across this picture in a design guide brochure for a 3D printing
service (Xometry). Immediately recognized the trochoid shape with
cooling chambers. I was going to inquire about the cost of the part and
whether dissimiliar metals can be combined in one cohesive part. Anyone
in the rotary group recognize it as their own?
Daniel Tyler
Inline image 1
Could they be making the part in wax or low temp plastic then casting
the housing? Wouldn't the housing be stronger if ot were cut from
billet? (Using a water jet cutter to avoid heating the metal ?
Rob Miller
Paul, Rob,
I have done a lot of research on the DMLS process. This is not wax! This
is directly FUSED metal. The resulting solid is generally as good as
billet material. This additive process uses the laser to melt the layers
together. many exotic materials are available. The earliest use I saw of
this technology was it make new shape jet engine compressor blades. This
is a very highly stressed part and the DMLS process was making a nearly
finished shape. Very little post machining. The price varies based on
how exact you want the part and the finish. If you want a very good
surface the layers must be very thin and the laser time will be high. If
you can deal with a fairly rough surface say +-.010-.015 it is
considerably cheaper. That rotor housing would require inside finishing
and coating, but the outside could be left as is. The water passages
might even benefit by having more surface area.
Bill Jepson
For turbine parts the material machining can be very expensive. If the
original
construction is very accurate there is almost no machining.
Dale Davies
According to someone I know who purchased a Lasertec DMLS a couple of
years ago from DMG Mori, the in-layer strength of DMLS is about equal to
a forged part. The between-layer strength is about like a cast part.
One big feature, aside from the ability to make quick corrections in a
model and then turn out an improved prototype, is the ability to mix
metals fairly freely within the part.
The side housing in the photo would be extremely expensive, even if one
owned a DMLS, because of the high cost of the powdered metal. A casting
would be much cheaper.
GE is now transitioning to ceramic matrix composites for their turbine
blades. As the price comes down for CMCs, I expect to see them in a lot
of applications, including automobile and aircraft reciprocating
engines. CMCs would be perfect for rotary engines, but right now the
price is just too high.
Dave Klingler
The Rotary Engine free News Letter. Powered by Linux. If you want off