12 c
Hi Paul,
This is the cush drive I have built for my single rotor.
It is machined out of 6061T6 billet on an old lathe and cheep
Chinese mill. The diameter is approx 4.7 inches, the inserts are
urethane rod at 1.25 inches in diameter. I am going to start with the
green urethane which is the lowest Shore hardness available here. the
photo shows a yellow grade which is slightly harder. The rod cuts
well with a sharp tungsten blade on a drop saw.
I have also had a new flywheel machined from billet 4140, as I was
not happy with the flex plate. The whole assembly has been
dynamically balanced.
Andrew Campbell.
Yes. That looks like it is going to work. Good idea. You should use
silicone rubber. Good to 500 F. There is a certain amount of energy
going into those dampers.
Urethane is only good to about 200 F.
Paul Lamar
Andrew, have you thought of selling those couplings? I think they
would sell well on this list. Craig . Smith
Found urethane to be unsuitable for my coushin drive, Lasted about 5
hours. Ended up with vulcanised rubber, so far brilliant!( 35
hours) . pictures of the urethane coupl;ings, As I said now done in
rubber and the price went up as usual.
Neil Unger,
--------------------------------------------------------------------------------------------
Please add your questions or comments at the end of the thread. Not
the beginning.
I am going to enforce that rule. If people don't do that it will not
be forwarded. My ISP changed the rules.
The Rotary Engine free News Letter. Powered by Linux. If you want
off the list PLEASE let me know and I will remove you. ACRE NL web
site.
http://www.rotaryeng.net <
http://www.rotaryeng.net/You Tube
http://tinyurl.com/beqqxas Copyright 1998-2017 All world wide rights
reserved.